Hardfacing Alloy #
6 |
|
| |
|
|
|
|
| |
|
Room Temperature |
600 deg C |
|
|
Typical Hardness RC |
38-48 |
30-37 |
|
|
|
|
|
|
|
Specifications |
|
|
|
American: |
AWS A5.13 RCoCr-A*, AWS A5.13
ECoCr-A*, AMS 5788 |
|
| |
|
MIL-R-17131, Type MIL-RCoCr-A-1 |
|
|
| |
European: |
DIN 8555: E20-UM-45-CRTZ |
|
|
| |
UNS: |
R30006, W73006 |
|
|
|
* Standard specification for this product. Other
specifications may be for similar products. |
| |
|
|
|
|
|
Description and Typical Usage |
|
| Deposit type & process - Cobalt
based deposit of Stellite 6 "type". Deposit via TIG, MIG, SMA,
or O-A.. |
|
| Properties - Very
resistant to metal-metal wear and to corrosion up to 800˚C.
Good resistance to thermal and |
|
|
mechanical shock. Good weldability. Resists galling in high load
metal-to-metal wear applications. |
|
| Typically used to hardface
- valves, valve seats, bearings, shafts, rotors, hot shear blades, hot
pressing tools, coke |
|
|
pulverizers, sintering parts, extrusion screws, etc. |
|
|
|
|
|
|
|
|
|
|
|
|
Nominal Chemistry - % |
|
|
|
(Main Classifying Elements Only) |
Sizes
Available |
|
| |
|
|
|
|
| |
Cobalt base with: |
|
Get
Quotation: Sales |
|
| |
C |
1.1 |
|
|
| |
Cr |
28 |
|
|
| |
W |
4 |
 |
|
| |
|
|
|
| |
|
|
|
| |
| Stellite® & Tribaloy® are
registered trademarks of Deloro Stellite. Stoodite® is a registered trademark of